ABSTRACT:A new diimide-diacid chloride (3) containing a noncoplanar 2,2Ј-dimethyl-4,4Ј-biphenylene unit was synthesized by treating 2,2Ј-dimethyl-4,4Ј-diamino-biphenylene with trimellitic anhydride followed by refluxing with thionyl chloride. Various new poly(ester-imide)s were prepared from 3 with different bisphenols by solution polycondensation in nitrobenzene using pyridine as hydrogen chloride quencher at 170°C. Inherent viscosities of the poly(esterimide)s were found to range between 0.31 and 0.35 dL g Ϫ1 . All of the poly(ester-imide)s, except the one containing pendent adamantyl group 5e, exhibited excellent solubility in the following solvents: N, N-dimethylformamide, tetrahydrofuran, tetrachloroethane, dimethyl sulfoxide, N,N-dimethylacetamide, N-methyl-2-pyrrolidinone, m-cresol, o-chlorophenol, and chloroform. The polymers showed glass-transition temperatures between 166 and 226°C. The 10% weight loss temperatures of the poly(ester-imide)s, measured by TGA, were found to be in the range between 415 and 456°C in nitrogen.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.