Gold flotation concentrate may contain relatively high concentrations of valuable metals such as iron, copper, and zinc, and occasionally, even precious metals such as gold. The major components of the concentrate are SiO 2 , Fe 2 O 3 , and Al 2 O 3 , but it also contains reactive sulphide minerals such as pyrite. The sulphides in the flotation concentrate are fully converted into an oxide form during oxidative roasting, therefore, the chemical composition of the roasted concentrate is considered to be a copper slag. High temperature smelting with additives to dissolve Au from the gold concentrate into a molten copper was used in the research. Gold greatly dissolved at 1600°С under a CaO/SiO 2 ratio of 1.25, suggesting the increase in the dissolution of gold into molten copper with decreasing viscosity of the molten slag-like concentrate at high temperatures.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.