The paper shows some physical properties of sessile oak obtained in Kosovo regions. In the study are shown: wood shrinkage, specific gravity, shrinkage coefficient for 1% change of moisture content, ratio of shrinkage in tangential and radial direction etc. The amount of volumetric shrinkage of sessile oak is 15.95%, heartwood part has an average shrinkage 15.41% in The shrinkage of sapwood part is 17.56%. Specific gravity at: wet condition: (1.013gr/cm3); 12% (0.853gr/cm3) and 0% (0.826gr/cm3) of moisture content. Specific gravity of heartwood at: wet condition (1.05gr/cm3); 12% (0.88gr/cm3); 0% (0.85gr/cm3). The specific gravity of sapwood at: wet condition (0.91gr/cm3); 12% (0.77gr/cm3); 0% (0.748gr/cm3). The ratio of average shrinkage between tangential and radial cutting direction is 1.71%. This ratio was significantly higher in sapwood than heartwood. Coefficient of shrinkage (changing 1% of moisture content) in the radial direction is 0.00196, and 0.00323 in tangential direction.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
customersupport@researchsolutions.com
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
This site is protected by reCAPTCHA and the Google Privacy Policy and Terms of Service apply.
Copyright © 2025 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.