We report a facile electrochemical route for the one-step fabrication of ZnO nanowire (NW) arrays. The method is seed-layer-free, and the NWs are directly attached to a fluorine-doped tin oxide (FTO) substrate. The effects of growth temperature, precursor concentration, substrate etching, and deposition time on the layer morphology and structure are analyzed. The ZnO NWs are vertically well-aligned and textured with the c-axis normal to the substrate. The growth of the more vertically oriented initial wires is favored by a self-alignment process, and the layer texturing with the c-axis oriented normal to the surface is increased upon deposition. NWs with aspect ratios higher than 30 have been synthesized. The as-grown layers were superhydrophilic, and they were converted to superhydrophobic by surface derivatization with stearic acid (SA). The surface could be commuted back from superhydrophobic to superhydrophilic by a simple acetone washing. The present work demonstrates the importance of oxide NW length to control the hydrophobic state of the surface. By increasing the NW length (and then the aspect ratio), a transition between a Wenzel state and a Cassie−Baxter state was found. For long and homogeneous ZnO NWs, the hysteresis is low (5.5°), and the advancing and receding contact angles are high (168.3°/162.8° max). The role of wire density is discussed. The superhydrophobic layers are of interest for self-cleaning surfaces, biological experiments, and nano/microfluidics.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.