Iron losses during calcium carbide based hot metal desulphurisation have been studied via large scale investigations of slag from the slag pit as well as slag sampling during desulphurisation at SSAB EMEA in Luleå . The desulphurisation slag, after injection of calcium carbide, is normally solid and contains large amounts of iron. An alkali containing mineral, nepheline syenite, was mixed together with the calcium carbide to form a more fluid slag as the iron losses originate from enclosed metal droplets in the slag as well as drawn off hot metal during slag skimming. The slag amount after slag skimming decreased from 28?1 to 25?1 kg t 21 hot metal with addition of 5 wt-% nepheline syenite to the calcium carbide, and the magnetic fraction of the slag from the slag pit decreased from 2?5 to 1?9%. Finally, no negative effect on the reagent efficiency was observed during the trials with addition of nepheline syenite.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.