Objective:The purpose of this study was to assess the microhardness of posterior composite resins at different depths varying the post-irradiation time.Materials and methods:For each composite resin [Solitaire 2 (SO) - Heraus Kulzer, P60 (P) - 3M, Prodigy Condesable (PC) - Kerr, Surefil (S) - Dentsply and Alert (A) - Pentron], 6 specimens (3 mm in diameter; 4mm high) were prepared using a black polyurethane cylindrical matrix. The resins were inserted in a bulk increment and light cured for 40 seconds. Microhardness was analyzed at different depths (top, 0.4 mm, 1.0 mm, 2.0mm, 3.0 mm and 4.0 mm) and at two moments (20 minutes and 24 hours after light-curing). Data were analyzed by ANOVA and Tukey's test (p<0.05).Results:Overall, microhardness means decreased significantly with the increase of depth, being lower in the first moment tested. P, S and PC showed the highest microhardness means.Conclusion:It may be concluded that the tested composite resins presented a gradual decrease of microhardness as depth increased and this drop was more accentuated for depths beyond 2 mm. For all materials, higher microhardness means were recorded 24 hours after light activation. P60 yielded the best results at the different depths evaluated.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
customersupport@researchsolutions.com
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
This site is protected by reCAPTCHA and the Google Privacy Policy and Terms of Service apply.
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.