In an acidic nitrate solution containing no less than 10 -4 mol/l Ag + , potentiostatic anodic dissolution of silver from its alloy with gold (up to 35 at. %) already in about 10 s is limited by the solid-phase mutual diffusion of the components. A number of diffusion-kinetic dissolution models taking into account contributions from the liquid-phase mass transfer, segregation in the surface layer, microroughness of the surface, shift of the alloy-solution interface, as well as the relaxation of nonequilibrium vacancies into a transient dissolution current are considered. The diffusivities and mutual diffusivities of the components, concentrations of nonequilibrium vacancies, and thickness of the diffusion zone estimated in terms of these models are compared. The effect of the overpotential and alloy composition is discussed. The main source of nonequilibrium monovacancies in the amount 14 orders as high as the equilibrium one is found to be the dissolution of silver. The efficiency of the sinks, among which the formation of bivacancies seemingly dominates, is not high, which predetermines the slowness of relaxation processes in the solid-phase diffusion zone. PROTECTION OF METALS Vol. 41 No. 4 2005 KOZADEROV et al .
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
customersupport@researchsolutions.com
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
This site is protected by reCAPTCHA and the Google Privacy Policy and Terms of Service apply.
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.