-In this research, 9 SAW welding specimens with 1 hour post-heat treatment (PH1) and 2 hours (PH2) were experimented to confirm the weldability and the joint performance of 60mm thickness HSA800 steel. SAW tests with PH1 & PH2, including weld impact test, bend test, hardness test, macroscopic test, and microscopic test, had a good test results. However, from the chemical composition test results, P composition was not satisfied with Korean Industrial Standards(KS). According to the weld-zone tensile tests, 2 hours post-heat SAW is recommended because the mechanical characteristics of SAW PH2 were better than those of SAW PH1. Keywords -HSA800, TMCP, SAW, Weldability, Welded joint performance, Post heat treatment, Homogeneity . 또한 용접부의 안전성은 주요 하중전달 부재 및 구조시스 템 간의 접합부에서 중요한 문제이며 [5] , 고강도·후판 강재 일수록 용접성능을 확보하는데 있어 용접재 설계, 용접사의 기 능도, 용접조건 등을 고려하여 종합적으로 검토하여야 한다.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.