Mn-Co and Cu-Mn based alloy coatings are deposited on 430 SS by high energy micro-arc alloying process, and then alloy coatings are oxidized at 750 ℃ in air to form the spinel oxides. Some composite oxides, such as Co3O4, Mn2O3 and (Mn,Co)3O4, are formed at the initial stage of oxidation. The single-phase spinel (pure MnCo2O4) without impurity phases is only found on the surface of Co-33Mn-17Cu oxide layer with the extended oxidation time, its area-specific resistance values at 500 ℃ to 800 ℃ are low and close to that of Mn-35Cu oxide layer which mainly composed of Cu1.2Mn1.8O4 spinel.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.