The present work analyzes possible increases in resistance to wear of nickel-titanium endodontic instruments that have undergone a process of ionic implantation. ProFile .04 taper #25 instruments were subjected to ionic implantation with bands of nitrogen ions of 250 KeV, currents in the order of 10 microA/cm2, and doses of 2 x 10(17) ions/ cm2. The instruments were used to make preparations in acrylic endodontic training blocks. Scanning electron microscopic investigations showed that after 60 s of work inside the endodontic training blocks nonionic implanted control instruments showed small modifications in their blades, and their tips showed the first signs of wear. After 240 s the control instruments showed consistent signs of wear and frequent changes to their surfaces. After 240 s of use the ionic-implanted instruments did not present any significant changes in the micromorphology of their surfaces. The implanted instruments did not manifest the typical signs of wear and did not show the surface changes that quickly affect the working life of untreated endodontic instruments manufactured from nickel-titanium.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.