A yellow inorganic ceramic pigment with general formula Y 1.86−x M x Tb 0.14 O 3−x/2 (M = Ca and/or Zn) with x = 0.06, 0.32 and 0.64 were synthesized by a modified Pechini method. XRD, SEM and HRTEM/EDX analysis showed the formation of solid solution at 1300 • C when x = 0.06 and 0.32. The best b* yellow coordinates were obtained for Ca and Zn co-doped Y 1.86 Tb 0.14 O 3 samples. The intensity of the yellow colour in the samples is related to the presence of Tb 4+ ions. Samples with higher concentration of Tb 4+ ions lead to a better yellow colour. The chemical stability of these pigments was determinate in an industrial glaze. The glazing tests indicated that the powder samples with x = 0.06 and 0.32 fired at 1300 • C were stable in the glaze. These results make it a potential candidate for environmental friendly yellow ceramic pigment to be used in applications such as pigment for glazes or inkjet printers.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.