Preparation and properties of La(Cr0.2Mn0.2Fe0.2Co0.2Ni0.2)O3 high-entropy ceramics are investigated. La(Cr0.2Mn0.2Fe0.2Co0.2Ni0.2)O3 high-entropy ceramics are prepared by a traditional two-step solid-state reaction method in air. La(Cr0.2Mn0.2Fe0.2Co0.2Ni0.2)O3 single-phase powders are synthesized by calcining the mixed oxides at 1000 °C for 20 h. The high-entropy ceramics are sintered at 1350–1650 °C in a muffle furnace for 4 h by using the above powders. The phase compositions of the high-entropy ceramics at different temperatures are characterized by X-ray diffraction (XRD) with Cu Kα radiation. A field-emission scanning electron microscope with energy-dispersive spectroscopy (EDS) is used to observe the microstructures and analyze the elemental distributions. The hardness and dielectric properties are measured and discussed.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.