“…CsCdBr 3 ) (for experimental lifetimes of ~0.096 ms in KPb 2 Cl 5 , ~1.57 ms in CsCdBr 3 and ~0.89 ms in Tl 3 PbBr 5 ). Despite similarly weak branching ratios in LaCl 3 crystals, laser operations at 5.2 and 7.2 m could be evidenced [Bowman et al, 1994[Bowman et al, , 1996. Utilizing a flash lamp pumped phosphate glass Kigre laser at 1.54 m, delivering pulse trains of 30 mJ at a frequency of 2 to 10 Hz, no luminescence issued from ( 3 F 4 , 3 F 3 ) multiplets at these two wavelengths could be observed in KPb 2 Cl 5 , CsCdBr 3 and Tl 3 PbBr 5 crystals.…”