“…A positive particularity of the reaction is the opportunity to carried out using easily available commercial reagents under soft conditions on the main laboratory equipment. In previously works we reported the results of studies, where both individual (butadiene rubber [14][15][16][17], styrene-butadiene rubber [18,19], nitrile-butadiene rubber [20]) polymers and polymer mixtures [21] were used as the initial matrix. The obtained products were successfully applied for the preparation of nanocomposites [21,22], adsorbents [23,24], and extractants for the concentration of metal ions by the solid phase extraction method [15,16,22].…”