Abstract:The diffusivity and activity coefficient of oxygen in liquid antimony, bismuth and antimony-bismuth alloys were determined from coulometric titration experiments, which were performed in the temperature range from 985 to 1185 K. The diffusivity in pure metals (in cm2/s) is: The standard free energy of solution of oxygen in liquid antimony, bismuth and antimony-bismuth alloys according to the reaction ½ O 2 (g) = O (infinite dilution) is calculated. The activity coefficient of oxygen was calculated at 1085 K as… Show more
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.