“…The structure of chalcogenide glass is mainly weakly covalently bonded chains made from bidentate chalcogen and cross-linked network formed by three or four ligand Ⅳ and Ⅴ elements, this relatively weak Vander Waals force between links leads to relatively poor mechanical properties, to some extent, limits the application of chalcogenide glass 6 . Micro-crystallization of glass can help to improve the mechanical performance of the chalcogenide glass through heat treatment and addition of nucleation agent, or combination of the two methods [7][8][9] . For example, Guo et al adds PbI in GeS 2 -Ga 2 S 3 to improve its mechanical hardness 10 .…”