Antireflection coating with enhanced anti-scratch property from nanoporous block copolymer template

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

0
19
0

Year Published

2013
2013
2018
2018

Publication Types

Select...
9

Relationship

0
9

Authors

Journals

citations
Cited by 28 publications
(19 citation statements)
references
References 20 publications
0
19
0
Order By: Relevance
“…Bicontinuous phases have attracted a lot of attention from the research community owing to their subtle microtextures and the easy control over the length scale. Nanomaterials with bicontinuous textures has been extensively exploited in different research areas, namely, optical applications, data storage, electronic devices, energy conversion and storage, mass transport, drug delivery systems, and catalysis . Also, there are many reviews well documenting the progress in these areas .…”
Section: Introductionmentioning
confidence: 99%
“…Bicontinuous phases have attracted a lot of attention from the research community owing to their subtle microtextures and the easy control over the length scale. Nanomaterials with bicontinuous textures has been extensively exploited in different research areas, namely, optical applications, data storage, electronic devices, energy conversion and storage, mass transport, drug delivery systems, and catalysis . Also, there are many reviews well documenting the progress in these areas .…”
Section: Introductionmentioning
confidence: 99%
“…A typical glass has a refractive index between 1.45 and 1.65 in the visible spectral region, which implies that the refractive index of an AR lm must be between 1.20 and 1.28. The silica AR lms [7][8][9][10] prepared by a sol-gel technique have been widely used in solar energy application elds for their low refractive index, ease of preparation and low cost. The growth of silica sols with an acid catalyzed sol-gel process invariably leads to a linear structure with branches.…”
Section: Introductionmentioning
confidence: 99%
“…The hardness is similar to that of a hard coating (no scratch until 2H) used in flat panel displays or touch panels. 28 MesoMSN-50 film 1 2 3 4 5 6 7 8 9 10 11 12 13 14 15 16 17 18 19 20 21 22 23 24 25 26 27 28 29 30 31 32 33 34 35 36 37 38 39 40 41 42 43 44 45 46 47 48 49 50 51 52 53 54 55 56 57 58 59 60 14 having cracks showed a variation in the data. The hardness of the reference coatings (MSN/PDMS) having interparticle voids was 2B even after calcination.…”
Section: Resultsmentioning