Atomic layer deposition of Ru nanoclusters on Ba–LaCeOx: a highly efficient catalyst for ammonia synthesis under mild conditions

Kaiying Wang,
Baitang Jin,
Xiaoqing He
et al.

Abstract: Ammonia synthesis has significant implications for global energy and environmental issues, driving the need for highly active catalysts that operate under mild conditions. This study reports the successful deposition of...