“…During the past decade, several approaches have been explored to tailor the magnetic properties of NiCuZn or NiZn ferrites and to lower their sintering temperatures, including using a variety of synthesis methods [6][7][8] and sintering conditions [9][10][11], adding dopants, such as SiO 2 , Bi 2 O 3 , La 2 O 3 , CoO, TiO 2 and MnO 2 [1,6,[12][13][14][15][16], and utilizing sintering aids, such as V 2 O 3 , Bi 2 O 3 and CaO-B 2 O 3 -SiO 2 [16][17][18]. These approaches have been mainly aimed at inducing changes in the densification mechanism of the ferrites so as to manipulate their microstructural evolution and grain boundary properties.…”