To perform a comparative study on curing shrinkage according to the thickness of photopolymerization resin.Methods: Stainless steel molds of 2, 4, and 6 mm heights were prepared. The 2, 4, and 6 mm-height molds were classified as the 2H, 4H, and 6H groups, respectively. A photopolymerization resin was injected into the stainless steel mold. Photopolymerization was carried out using a photopolymer machine. During photopolymerization, the wavelength and intensity of 400~405 nm were set to 10, the highest intensity among 1~10. Photopolymerization was performed for 30 min per specimen (each group=10). The inner and outer areas of the specimen were measured. The data were analyzed using one-way ANOVA and Kruskal-Wallis H test (α=0.05).Results: In terms of the inner and outer diameters of the photopolymerization resin specimen, the 2H group contracted the most, whereas the 6H group contracted the least. A statistically significant difference was found between the groups (p<0.05).
Conclusion:The amount of light irradiation of the photopolymerization resin must be adjusted according to the thickness.