Abstract:Electrode degradation in continuous resistance spot welding process of BH 220 steel was evaluated by electrode life test, and weldability tests were conducted by geometry features measurement, mechanical property analysis, and electrode diameter measurement with 88 or 176 weld intervals. The analysis of weld geometry shows that the HAZ width, nugget diameter, and nugget area tend to decrease rapidly, while the nugget height tends to firstly increase with the weld repetitions till the welding heat input becomes… Show more
Set email alert for when this publication receives citations?
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.