Effect of light-emitting diode and halogen light curing on the micro-hardness of dental composite and resin-modified glass ionomer cement: An in vitro study

Abstract: It was concluded that the curing efficacy of the LED lamp was comparable to that of conventional halogen lamp, even with a 50% reduction in cure time, and resin composite (Filtek Z-250) presented the highest hardness values, whereas complete hardening of resin-modified glass ionomer cement (RMGIC) (Vitremer) was observed because of its self-curing system even after the removal of light source.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

0
6
0
6

Year Published

2013
2013
2021
2021

Publication Types

Select...
4
1
1

Relationship

0
6

Authors

Journals

citations
Cited by 9 publications
(12 citation statements)
references
References 0 publications
0
6
0
6
Order By: Relevance
“…El ionóme-ro de vidrio es uno de los materiales más utilizados en el área de rehabilitación oral, y actualmente es el material de elección como base intermedia debido a su adhesión a la estructura dentaria y a su efecto anticariogénico, además de su comportamiento mecánico [1][2][3][4][5]. Su elevado módulo elástico y su coeficiente de expansión térmica son similares a los de la dentina, lo que le da una rigidez similar a ella [6][7][8].…”
Section: Introductionunclassified
See 1 more Smart Citation
“…El ionóme-ro de vidrio es uno de los materiales más utilizados en el área de rehabilitación oral, y actualmente es el material de elección como base intermedia debido a su adhesión a la estructura dentaria y a su efecto anticariogénico, además de su comportamiento mecánico [1][2][3][4][5]. Su elevado módulo elástico y su coeficiente de expansión térmica son similares a los de la dentina, lo que le da una rigidez similar a ella [6][7][8].…”
Section: Introductionunclassified
“…Los ionómeros de vidrio presentan una alta susceptibilidad a la humedad debido a su proceso de endurecimiento, el cual tiene una maduración inicial durante las primeras 24 horas [1][2][3][4][5][6][7][8][9][10][11][12][13][14].…”
Section: Introductionunclassified
“…1 In hybrid ionomer, water-soluble methacrylate-based monomers have been used to replace part of liquid component of conventional glass ionomer cement. in attempt to improve mechanical properties, decrease setting time, and reduce moisture sensitivity of glass ionomer materials.…”
Section: Introductionmentioning
confidence: 99%
“…Entretanto, os CIVs são materiais friáveis e porosos (Talal et al, 2009;Azevedo et al, 2011) e bastante sensíveis à umidade, sofrem sinérese ou embebição antes da maturação, especialmente nas primeiras 24 horas, podendo ocorrer dissolução ou trincas no material, comprometendo algumas propriedades como resistência inicial do material, dureza e resistência ao desgaste (CattaniLorente et al, 1999;Talal et al, 2009;Azevedo et al, 2010;O'Brien et al, 2010;Azevedo et al, 2011;Guglielmi et al, 2012;Fabián Molina et al, 2013;Calvo et al, 2016 (Yiu et al, 2004a;Xie et al, 2008;Kim et al, 2013 (Yiu et al, 2004b;Talal et al, 2009;O'Brien et al, 2010;Arita et al, 2011;Bhalla et al, 2012;Guglielmi et al, 2012;Pacifici et al, 2014), além disso há relatos de problemas toxicológicos devido a liberação de monômeros pelo CIVMR ,o que pode irritar a polpa dentária restringindo o uso desse material em alguns casos (Kleverlaan et al, 2004;Xie et al, 2008;Talal et al, 2009;Azevedo et al, 2010).…”
Section: Características Dos Cimentos De Ionômero De Vidrounclassified
“…As a result the FS, the ultrasound with setting reaction resulted in higher values and similar to the negative control group, regardless of the format of the HVGIC. SR for Ra (Hse et al, 1999;da Silva;Zuanon, 2006;Frencken, 2010;Bhalla et al, 2012) mostrando longevidade satisfatória em restaurações oclusais (Frencken et al, 2004;Faccin et al, 2009;Frencken, 2010;Mickenautsch et al, 2010;Fábian Molina et al, 2013) e, até mesmo ocluso-proximais, quando comparados a outros materiais (Raggio et al, 2013 (Frencken et al, 2004;da Silva;Zuanon, 2006;Frencken, 2010).…”
Section: Introductionunclassified