“…Furthermore, the observed F K-edge XAS spectra look distinct from those of magnesium fluorides [38] and iron fluorides [39], indicating the absence of interlayer mixing between the Fe, LiF, and MgO layers. Despite the spectral overlap between F K-edge and Fe L 2,3 -edge XAS spectra, we subtracted backgrounds in a rather standard way [40]; we subtracted the summation of a double step function and a linear function that bends at the Fe L 3 edge such that XAS intensities become zero in the pre-edge (around 700 eV) and post-edge regions (around 740 eV). The backgrounds are shown by solid curves separately for each spectrum in Fig.…”