Enabling Large Superalloy Parts Using Compact Coprecipitation of γ′ and γ′′

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1

Citation Types

6
28
0

Year Published

2018
2018
2024
2024

Publication Types

Select...
5
2
1

Relationship

0
8

Authors

Journals

citations
Cited by 61 publications
(34 citation statements)
references
References 18 publications
6
28
0
Order By: Relevance
“…Concluded from above results, γ ′ phase can provide APB‐shearing induced ordered strengthening effects on yield strength for Inconel 718 alloy. In the modified compact configuration with γ ″ phase reported by some works, the γ ′ deformation behavior may be modified by adjacent γ ″, in turn, the γ ″ deformation is also influenced by neighboring γ ′. For this case, understanding the cooperative deformation mechanisms of γ ″ and γ ′ is necessary for design of newly bimodal γ ″‐ γ ′ hardened 718‐type alloys, which should attract more research attentions.…”
Section: Resultsmentioning
confidence: 98%
See 1 more Smart Citation
“…Concluded from above results, γ ′ phase can provide APB‐shearing induced ordered strengthening effects on yield strength for Inconel 718 alloy. In the modified compact configuration with γ ″ phase reported by some works, the γ ′ deformation behavior may be modified by adjacent γ ″, in turn, the γ ″ deformation is also influenced by neighboring γ ′. For this case, understanding the cooperative deformation mechanisms of γ ″ and γ ′ is necessary for design of newly bimodal γ ″‐ γ ′ hardened 718‐type alloys, which should attract more research attentions.…”
Section: Resultsmentioning
confidence: 98%
“…Axter and Polonis supposed that the high‐energy faults formed within γ ′ phase during deformation may result in the increase of yield strength for bimodal γ ″‐ γ ′ hardened alloy. In progress, recent trials by Detor et al, Mignanelli et al have proved the superior temperature capability benefited from the co‐precipitation of comparable γ ′ and γ ″ phase, and therefore refocused attentions to the underestimated thermal stabilizing role of γ ′ phase in the bimodal γ ″‐ γ ′ configuration.…”
mentioning
confidence: 99%
“…the Al/Ti ratio along with (Al + Ti)/Nb atomic ratio in IN718, a more thermally and mechanically stable co-precipitate γ ′′ /γ ′ microstructure can be also achieved, which could be due to a higher volume fraction of γ ′ or the smaller γ ′′ precipitate sizes [16]. Such a slow coarsening effect of co-precipitation of γ ′′ /γ ′ also provides a promising solution to avoid the overageing of γ ′ -strengthened disk alloys during processing [17,18]. There is possibly another way to minimize the coarsening of γ ′′ by tailoring its variants.…”
Section: Inconel 718mentioning
confidence: 99%
“…Table I shows the nominal composition of IN718 and a derivative IN718M without γ forming elements. Recent studies aim at deliberate co-precipitation of γ and γ to exploit ripening inhibiting effects [6,7] and a dual lattice microstructure [8,9]. IN718 powders also gain importance for additive manufacturing in the industrial environment [10][11][12][13].…”
Section: Introductionmentioning
confidence: 99%