“…For example, Inoue et al have prepared a series of Al-Cu-Y metallic glasses within the composition range of 3-22 at% Y by melt spinning and found that when the Al content is more than 80 at%, the metallic glasses have good bend ductility [20,21]. Fukunaga et al, have obtained Alx(Cu0.4Y0.6)100−x (x = 0, 5, 10, 15, 20, 30, 80, and 85) metallic glasses by arc melting and further studied their atomic and electronic structures [31]. In addition, Idzikowski et al have obtained fully amorphous Al8Cu42Y50 ribbon by melt-spinning and further tracked its structural evolution with varying annealing time [32].…”