“…When adding SiO 2 and Na 2 CO 3 , the reaction temperature of apatite decreased, which promoted the reduction reaction to generate phosphorus-containing gas. 16) In addition, CaO, SiO 2 , Al 2 O 3 , and Na 2 CO 3 interacted to form Na 2 CaSi 5 O 12 and NaAlSiO 4 phases with a low melting point. The formation of low melting point compounds improved the fluidity of the system and destroyed the inclusion structure of gangue relative to apatite in the ore, therefore the reduction reaction of apatite proceeded better.…”