“…Very high heating rates, approaching 20.000°C/min, can be therefore achieved [200]. his technology was successfully applied to B 4 C and SiC/B 4 C composites which were sintered in about 3 s. Moreover, specific microstructures are developed upon contactless flash sintering, among them platelets SiC crystals those growth has been attributed to physical vapor transport mechanisms [201].…”