“…6c), which is higher than those of most reported ASCs and materials. 10,19,20,[43][44][45][46][47][48] Meanwhile, the ASC delivers a volumetric energy density of 114.3 W h L −1 at a volumetric power density of 517.9 W L −1 (Fig. 6d), superior to many advanced ACSs and materials, including HRGO/Ni(PA) 2 -1//HRGO (23.7 W h L −1 at 632 W L −1 ), 49 GO (9.1 W h L −1 at 2777.3 W L −1 ), 50 CLFW@(Co, Ni)-(CoS, NiS) (66 W h L −1 at 50 W L −1 ), 51 CNF@Ni (58 W h L −1 at 39 W L −1 ), 52 and GNS/Fe (14.6 W h L −1 at 381 W L −1 ).…”