Improve stress corrosion cracking resistance and mechanical properties of Al‐Zn‐Mg‐Cu‐Zr alloy with heterogeneous lamellae structure produced by high pressure torsion
Abstract:High pressure torsion experiment followed with heat treatment were carried out on as‐cast Al‐Zn‐Mg‐Cu‐Zr alloy at 400 °C under the pressure of 1 GPa. The microstructure, mechanical property and stress corrosion resistance properties for the as‐cast and high pressure torsion processed samples were studied. The results show that high pressure torsion processing can improve the mechanical property by the refinement of grains and grain boundary precipitates, as well as the homogeneous distribution of fine matrix p… Show more
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.