“…There is a singular grain growth for all the ceramics after sintered at T s2 . The average grain size, which belongs to coarse-grained category [7], is 40 m, 20 m, 30 m and 10 m for the Ba (1−x) Sr x TiO 3 ceramics at x = 0, x = 0.01, x = 0.02 and x = 0.03, respectively. With the sintered temperature rising to T s3 , the grain size of the Ba (1−x) Sr x TiO 3 ceramics at x = 0, x = 0.01, x = 0.02 and x = 0.03 increase to 50 m, 50 m, 40 m and 30 m, respectively.…”