Influence of pH on structural, morphological and optical properties of chemically deposited nanocrystalline ZnO thin films

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
6
0

Year Published

2017
2017
2024
2024

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 8 publications
(6 citation statements)
references
References 28 publications
0
6
0
Order By: Relevance
“… 46 This structure is part of the space group C 4 6 v in the Schoenflies notation and P 6 3 mc in the Hermann–Mauguin system and exhibits a noncentrosymmetric structure (a condition at where the space groups lack inversion center). 46 At ambient conditions, only the wurtzite structure has a thermodynamically stable hexagonal unit cell, 44 wherein four oxygen atoms surround each tetrahedral Zn atom and vice versa ( 47 )…”
Section: Resultsmentioning
confidence: 99%
See 2 more Smart Citations
“… 46 This structure is part of the space group C 4 6 v in the Schoenflies notation and P 6 3 mc in the Hermann–Mauguin system and exhibits a noncentrosymmetric structure (a condition at where the space groups lack inversion center). 46 At ambient conditions, only the wurtzite structure has a thermodynamically stable hexagonal unit cell, 44 wherein four oxygen atoms surround each tetrahedral Zn atom and vice versa ( 47 )…”
Section: Resultsmentioning
confidence: 99%
“…ZnO is known to occur in three crystal (lattice) structures viz. rock-salt (B 1 ), cubic zinc-blende (B 3 ), and wurtzite (B 4 ). , The zinc-blende shape is stabilized by hetero-epitaxial expansion on cubic substrates, for example GaAs/ZnS, ZnS, and Pt/Ti/SiO 2 /Si, while the structure of the Rochelle salt/rock salt (NaCl) is a metastable state reached at high pressure only. Wurtzite ZnO is a hexagonal crystal having lattice parameters “ a ” and “ c ” and a lattice constant ( c / a ) of (1:633, in a typical wurtzite hexagonal structure), with [0 0 0 1] or basal plane as the surface most frequently used for growth .…”
Section: Resultsmentioning
confidence: 99%
See 1 more Smart Citation
“…080-0075, Te International Centre for Difraction Data, PA, USA). Tree crystal lattice confgurations of ZnO are known to exist: wurtzite (B4), cubic zincblende (B3), and rock salt (B1) [39,40]. Only heteroepitaxial formation on cubic platforms, such as ZnS, GaAs/ZnS, and Pt/Ti/SiO2/Si, can maintain the zinc-blende type, whereas elevated pressure is required to produce the metastable rock salt or Rochelle salt (NaCl) form.…”
Section: Structural Properties Of Synthesized G-zno Npsmentioning
confidence: 99%
“…As the pH increases from 7.5 to 10.5, through 8.5 and 9.5 the value transmittance percentage increases. [15][16][17][18] …”
Section: Fig 3:-absorption Spectra Of Zno Nanorods At Different Ph Vmentioning
confidence: 99%