The La0.7SrxCa0.3-xMnO3 (x=0, 0.05, 0.1, 0.15, 0.2, 0.25 and 0.3) were prepared by combining sol-gel method and high temperature sintering. The effects of Sr doping content on the structure and morphologies of the La0.7SrxCa0.3-xMnO3 finally sintered at 1050°C/1250°C were investigated based on the analyses of X-ray diffraction (XRD) and Scanning Electron Microscope (SEM). The results show that the La0.7SrxCa0.3-xMnO3 exhibit single perovskite phase and the change of Sr doping content can result in phase structure transition. The La0.7SrxCa0.3-xMnO3 samples are rhombohedra structure in the range of 0.15≤x≤0.3. When x is no more than 0.1, the La0.7SrxCa0.3-xMnO3 samples sintered at 1050°C present distorted cubic structure. The microstructure of La0.7SrxCa0.3-xMnO3 sintered at 1050°C for 5h becomes more and more looser and its grains tend to refinement with the increase of Sr doping content when x is no less than 0.05. Increasing the final sintering temperature can improve the density and promote the grain growth of La0.7SrxCa0.3-xMnO3. In order to gain a dense microstructure, the final sintering temperature of La0.7SrxCa0.3-xMnO3 should be higher than 1050°C and should be suitably increased with the increase of Sr doping content.