“…Also, the peaks were shied when milling for up to 5 h, signifying the presence of atomic disorder and accumulated strain during the material synthesis. 29 However, for t mill ¼ 10 h, signicant intense peaks of TiO 2 and Ni could be observed at the expense of the NiO peaks, indicating the considerable reduction of NiO. This resulted in the formation of in situ NiO-Ni-TiO 2 nanocomposites.…”