Mechanical Fractography and Worn Surface Analysis of Nanographite and ZrO2-Reinforced Al7075 Alloy Aerospace Metal Composites

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
5
0

Year Published

2021
2021
2024
2024

Publication Types

Select...
9

Relationship

1
8

Authors

Journals

citations
Cited by 23 publications
(8 citation statements)
references
References 17 publications
0
5
0
Order By: Relevance
“…Moreover, wear is mild oxidative at lower load and changed to metallic wear at high load values. Many authors in literature have observed similar kinds of behavior between wear loss and normal load for AA5052/zirconium diboride, AA7075/molybdenum disulfide/tri silicon tetranitride, and aluminum/silicon carbide/molybdenum disulfide composites respectively [2,23,40,41,42].…”
Section: Effect Of Normal Loadmentioning
confidence: 66%
“…Moreover, wear is mild oxidative at lower load and changed to metallic wear at high load values. Many authors in literature have observed similar kinds of behavior between wear loss and normal load for AA5052/zirconium diboride, AA7075/molybdenum disulfide/tri silicon tetranitride, and aluminum/silicon carbide/molybdenum disulfide composites respectively [2,23,40,41,42].…”
Section: Effect Of Normal Loadmentioning
confidence: 66%
“…In particular, the ideal hardness of reinforced composites featuring a mixture surpasses the hardness of unreinforced alloys. This rise in hardness can be attributed to the increased occurrence of hard SiO2 particles in the aluminum matrix, combined with the inherently high hardness of nano graphene particles [40]. The introduction of reinforcement particles to the aluminum matrix serves to enhance their surface area, concurrently reducing the size of aluminum matrix grains.…”
Section: Hardness Measurementsmentioning
confidence: 99%
“…Al7010 alloy and 20-25 micron sized B 4 C composites wear behavior at varying speeds of 0.60 m/s to 2.40 m/s at constant load of 40 N for 3000 m sliding distance is shown in Figure 13. A delamination in the Al7010 alloy has caused fragments of pins to be transferred to the disc, while larger pieces have been ejected [25,26]. Wear is decreased when B 4 C is combined with Al7010.…”
Section: Effect Of Sliding Velocity On Volumetric Wear Lossmentioning
confidence: 99%