Novel cattail fiber composites: converting waste biomass into reinforcement for composites

Abstract: Vacuum-assisted resin transfer molding (VARTM), used in manufacturing medium to large-sized composites for transportation industries, requires non-woven mats. While non-woven glass mats used in these applications are optimized for resin impregnation and properties, such optimized mats for natural fibers are not available. In the current research, cattail fibers were extracted from plants (18–30% yield) using alkali retting and non-woven cattail fiber mat was manufactured. The extracted fibers exhibited a norma… Show more

Help me understand this report
View preprint versions

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1

Citation Types

1
16
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
6

Relationship

2
4

Authors

Journals

citations
Cited by 11 publications
(17 citation statements)
references
References 29 publications
1
16
0
Order By: Relevance
“…6H 2 O], 75.5% (NaCl), 84.3% (KCl), 93.6% (KNO 3 ) and 100% (H 2 O) according to ASTM D 1776-4 (2008). Before conditioning, WBFs were dried in an oven at 100 C for 12 h. The MC(%) was calculated as a percentage of the ratio of the weight of water absorbed by the sample to the total weight of the sample as expressed in equation (1). where M w is the weight of samples after conditioning and M 0 is the weight of water in samples.…”
Section: Measurement Of Moisture Contentmentioning
confidence: 99%
See 4 more Smart Citations
“…6H 2 O], 75.5% (NaCl), 84.3% (KCl), 93.6% (KNO 3 ) and 100% (H 2 O) according to ASTM D 1776-4 (2008). Before conditioning, WBFs were dried in an oven at 100 C for 12 h. The MC(%) was calculated as a percentage of the ratio of the weight of water absorbed by the sample to the total weight of the sample as expressed in equation (1). where M w is the weight of samples after conditioning and M 0 is the weight of water in samples.…”
Section: Measurement Of Moisture Contentmentioning
confidence: 99%
“…5965, Sl# VS02075661, manufactured by Instron, Norwood, USA) following the ASTM D3822 method and the procedure described in Shadhin and colleagues (2021). 1,2 The capacity of the load cell used for this study was 1 kN. The tensile testing setup with the fiber frames between the serrated grips in Instron is illustrated in Figure 1(g).…”
Section: Measurement Of Mechanical Propertiesmentioning
confidence: 99%
See 3 more Smart Citations