2007
DOI: 10.1039/b615104c
|View full text |Cite
|
Sign up to set email alerts
|

Oxide ion conduction in Ba, Ca and Sr doped apatite-type lanthanum silicates

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

2
61
0
2

Year Published

2010
2010
2023
2023

Publication Types

Select...
8

Relationship

0
8

Authors

Journals

citations
Cited by 59 publications
(65 citation statements)
references
References 31 publications
2
61
0
2
Order By: Relevance
“…In contrast, alkaline earth (Ca, Sr, Ba) doped samples containing oxygen excess all exhibited high oxide conductivities (e.g. s at 700 C ¼ 8.74 Â 10 À3 S cm À1 for La 9 Sr(SiO 4 ) 6 O 2.5 , versus 3.26 Â 10 À4 S cm À1 for La 9.33 , 0.67 Si 6 O 26 ) [22]. These results also show that oxygen excess is more important than cationic vacancies to achieve good oxide-ion conductivity of lanthanum silicate oxyapatite.…”
Section: Introductionmentioning
confidence: 89%
“…In contrast, alkaline earth (Ca, Sr, Ba) doped samples containing oxygen excess all exhibited high oxide conductivities (e.g. s at 700 C ¼ 8.74 Â 10 À3 S cm À1 for La 9 Sr(SiO 4 ) 6 O 2.5 , versus 3.26 Â 10 À4 S cm À1 for La 9.33 , 0.67 Si 6 O 26 ) [22]. These results also show that oxygen excess is more important than cationic vacancies to achieve good oxide-ion conductivity of lanthanum silicate oxyapatite.…”
Section: Introductionmentioning
confidence: 89%
“…The cationic substitutions on the La site with other rare earth elements [15e17] or alkaline earth elements [18e23] have been investigated. The samples containing oxygen excess exhibit high oxygen ion conductivity, which indicates that oxygen excess is more important than cationic vacancies to achieve good oxide-ion conductivity of oxy-apatite lanthanum silicate [21].…”
Section: Introductionmentioning
confidence: 99%
“…The intensity of the La 2 SiO 5 second phase of LCSFO(SSP) is lower than that of LSFO(SSP) synthesized under identical conditions and temperatures, indicating that doping Ca on the La site for LSFO oxyapatite can further retard the formation of the La 2 SiO 5 secondary phase. However, as shown previously, phase pure lanthanum silicate apatite-type powders synthesized by SSP can be formed at temperature above 1500 C [29,41]. Fig.…”
Section: Phase and Microstructure Of The Oxyapatitesmentioning
confidence: 82%
“…Fig. 1c is the XRD patterns of LCSFO powders synthesized by SGP at the temperatures of 700e1000 C. The oxyapatite phase starts to form at 700 C and the complete formation of apatite phase for LCSFO(SGP) powders occurs at 750 C. This is substantially lower than complete phase formation temperature of~1500 observed for the lanthanum silicates such as La 10 Si 6 O 27 and La 9 Ba 1 Si 6 O 26.5 synthesized by SSP route [29,41]. La 2 SiO 5 was not detected.…”
Section: Phase and Microstructure Of The Oxyapatitesmentioning
confidence: 95%
See 1 more Smart Citation