“…For the fabrication of flexible films containing encapsulated Sb 2 Te 3 -MWCNT or bare MWCNTs, the heterostructures were deposited on polyimide substrates, then coated with PDMS (Sigma-Aldrich, Inc., St. Louis, MI, USA), cured for 10 min in 150 °C, and then the resulting elastic film was lifted off the glass using tweezers. For the fabrication of mixed composite, the Sb 2 Te 3 -MWCNT heterostructures were deposited on glass substrates, then scrapped off the substrates and mixed in PVA (Sigma-Aldrich, Inc., St. Louis, MI, USA) as described elsewhere [ 13 ].…”