Poly-Lactide/Exfoliated C30B Interactions and Influence on Thermo-Mechanical Properties Due to Artificial Weathering

Abstract: Thermal stability as well as enhanced mechanical properties of poly-lactide (PLA) can increase PLA applications for short-use products. The conjunction of adequate molecular weight (M W ) as well as satisfactory thermo-mechanical properties, together, can lead to the achievement of suitable properties. However, PLA is susceptible to thermal degradation and thus an undesired decay of M W and a decrease of its mechanical properties during processing. To avoid this PLA degradation, nanofiller is incorporated as r… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
1
0

Year Published

2017
2017
2021
2021

Publication Types

Select...
5

Relationship

0
5

Authors

Journals

citations
Cited by 6 publications
(1 citation statement)
references
References 31 publications
(37 reference statements)
0
1
0
Order By: Relevance
“…The optimization of this process is, however, challenging regarding nanolevel dispersion of particles and ensuring structural integrity of the nanofillers . Apart from that, the processing method and temperature regime should have minimal adverse effects on the PLA matrix which is prone to degradation above 180 °C …”
Section: Introductionmentioning
confidence: 99%
“…The optimization of this process is, however, challenging regarding nanolevel dispersion of particles and ensuring structural integrity of the nanofillers . Apart from that, the processing method and temperature regime should have minimal adverse effects on the PLA matrix which is prone to degradation above 180 °C …”
Section: Introductionmentioning
confidence: 99%