“…The optimum values for the parameters were reported as 2.5% biomass loading, 6 h time, and 100°C temperature. Muley et al [77] used microwave-assisted delignification for the treatment of pinewood sawdust. Three different DESs, namely, ChCl-oxalic acid (1:1), ChCllactic acid (1:1), and ChCl-formic acid (2:1), were used to test the effect of temperature (110, 130, and 150°C) and time (1, 5, 10, and 15 min) at 2450 MHz.…”