The processes of pyrolysis and combustion of rubber-based synthetic rubbers were studied. Determined that Teflon (polytetrafluoroethylene) helps reduce the rate of burning rubber in half, from 0.25 mm/s to 0.14 m/s based on a mixture of isoprene and butadiene-styrene rubbers