“…The hard segment of thermoplastic PU elastomers can form a thermotropic liquid‐crystalline phase when properly selected and when diisocyanate and chain extender are used for polyaddition reaction. The hard segments prepared from 4,4′‐dihydroxybiphenyl (DHBP)/hexamethylene diisocyanate (HDI),16 4,4′‐bis(6‐hydroxyhexoxy)biphenyl (BHHBP)/4,4′‐diphenylmethane diisocyanate (MDI),17 4,4′‐bis(2‐hydroxyethoxy)biphenyl/toluene diisocyanate (TDI),18 and BHHBP/TDI19 pairs are examples of thermotropic liquid‐crystalline PUs. Furthermore, to balance the mesogenic properties and elastic nature of PU, Padmavathy and Srinivasan20 used a high‐aspect‐ratio, tetrad, hexyloxy spacer, mesogenic diol as a chain extender.…”