“… methods | year, author and reference | tube size and material | film material and thickness |
PVD | 1992, J. A. Sheward [ 5 ] | Ø120 mm, steel | Cr-Nb, 7–17 µm |
2016, D. Kottfer [ 7 ] | Ø200–300 mm, steel | Ti, 1.3–3.9 µm |
CVD | 1986, H. Itoh [ 10 ] | Ø10 mm, steel | TiN, 12 µm |
2013, H. Kousaka [ 9 ] | Ø4.4 mm, steel | DLC, 529 nm |
2014, R. Hatada [ 11 ] | Ø25 mm, steel | Ag-DLC, 150 nm |
2017, Y. Xu [ 8 ] | Ø0.9 mm, glass and lucalox | DLC, -- |
electroplating | 2014, L. D. Sun [ 13 ] | Ø9 mm, Ti | TiO 2 , 5–15 µm |
2017, C. J. Xiang [ 12 ] | Ø10 mm, Ti | TiO 2 , 0.1–1 µm |
electrical explosion | 2000, O. Demokan [ 15 ] | Ø13 mm, Ta | Al, 7.1–8.1 µm |
dip-coating | 2007, W. C. Gu [ 17 ] | Ø50 mm, steel | ceramic, 300 µm |
2018, S. Ayata [ 18 ] | Ø16 mm, Al-Cu-Mg | ZrO 2 -DLC, 182 nm |
…”