Abstract: Traditional means of core fabrication are to glue the laminations or weld them to form the yoke structure. These means result in good yoke assemblies for shorter (<0.6 meter) magnets. However, because of weld distortions or mechanical strength limitations, welding and/or gluing techniques result in cores with poor mechanical precision or limited mechanical strength for longer cores. The SPEAR3 gradient dipole magnets are up to 1.45 meters long and require distortions of <0.05 mm. Therefore, the SPEAR3 gradient… Show more