“…[16] Unfortunately, it is not possible to compare the strength directly, due to different measuring geometry, sample geometry (size, relative density, cell size), or other missing measurement parameters. [7,16,18] The Weibull moduli m range from 1.9 to 5.7 and exhibit no obvious correlation to varied parameters (T max1 , T max2 , colloid, infiltration technique; Table 2). The scattering range suggests an influence of the sample preparation, but differences in preparation were not identified, and the Weibull moduli as calculated are in the range as reported for comparable cellular materials.…”