2023
DOI: 10.1016/j.cej.2023.143324
|View full text |Cite
|
Sign up to set email alerts
|

Structural tailoring enables ultrahigh energy density and charge–discharge efficiency of PAEK copolymer dielectrics at high temperatures

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

0
4
0

Year Published

2023
2023
2024
2024

Publication Types

Select...
7

Relationship

1
6

Authors

Journals

citations
Cited by 19 publications
(4 citation statements)
references
References 40 publications
0
4
0
Order By: Relevance
“…Polymer dielectrics that maintain a consistent dielectric constant and exhibit low dielectric loss across an extensive range of frequencies and temperatures are essential prerequisites for the practical application of commercial capacitors. As shown in Figure b, the β-relaxation peak of the PPES has appeared at higher temperatures (over 150 °C), and this is caused by the rotation of small-sized dipoles of nitrogen atoms of the nitrogen-containing heterocyclic ring of the phthalazinone moiety Figure c shows that a minor variation in ε r and tan δ values against temperature (25–200 °C) at different frequencies (10 2 to 10 6 Hz) is seen in PPES films.…”
Section: Resultsmentioning
confidence: 90%
See 1 more Smart Citation
“…Polymer dielectrics that maintain a consistent dielectric constant and exhibit low dielectric loss across an extensive range of frequencies and temperatures are essential prerequisites for the practical application of commercial capacitors. As shown in Figure b, the β-relaxation peak of the PPES has appeared at higher temperatures (over 150 °C), and this is caused by the rotation of small-sized dipoles of nitrogen atoms of the nitrogen-containing heterocyclic ring of the phthalazinone moiety Figure c shows that a minor variation in ε r and tan δ values against temperature (25–200 °C) at different frequencies (10 2 to 10 6 Hz) is seen in PPES films.…”
Section: Resultsmentioning
confidence: 90%
“…As shown in Figure 2b, the β-relaxation peak of the PPES has appeared at higher temperatures (over 150 °C), and this is caused by the rotation of small-sized dipoles of nitrogen atoms of the nitrogen-containing heterocyclic ring of the phthalazinone moiety. 28 Figure 2c shows that a minor variation in ε r and tan δ values against temperature (25−200 °C) at different frequencies (10 2 to 10 6 Hz) is seen in PPES films. However, as shown in Figure 2d, it is evident that the tan δ of PSF is raised over 180 °C.…”
Section: Dielectric Propertiesmentioning
confidence: 96%
“…P(AEK-BBP) (with 15 mol% of BBP) was prepared according to our previously work. 39 Preparation of the m -ABA-BN nanoparticles…”
Section: Methodsmentioning
confidence: 99%
“…The resulting c -P(AEK-BBP) copolymer exhibits excellent thermal stability, mechanical properties, and dielectric performance. 39…”
Section: Introductionmentioning