2019
DOI: 10.1007/s11665-019-03913-7
|View full text |Cite
|
Sign up to set email alerts
|

Sulfide Stress Corrosion Cracking Behavior of G105 and S135 High-Strength Drill Pipe Steels in H2S Environment

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

0
6
0

Year Published

2021
2021
2024
2024

Publication Types

Select...
9

Relationship

1
8

Authors

Journals

citations
Cited by 13 publications
(6 citation statements)
references
References 24 publications
0
6
0
Order By: Relevance
“…Furthermore, the bonding force between metal atoms weakens, reducing external stress required for crack propagation and increasing material cracking sensitivity. Therefore, under the action of external stress or residual stress of the weld at both ends of the pipeline, the pipeline was most prone to cracking and damage at weak points [23][24][25]. Based on the above analysis, it was concluded that the pipeline fracture was caused by sulfide stress corrosion cracking.…”
Section: Comprehensive Analysismentioning
confidence: 99%
“…Furthermore, the bonding force between metal atoms weakens, reducing external stress required for crack propagation and increasing material cracking sensitivity. Therefore, under the action of external stress or residual stress of the weld at both ends of the pipeline, the pipeline was most prone to cracking and damage at weak points [23][24][25]. Based on the above analysis, it was concluded that the pipeline fracture was caused by sulfide stress corrosion cracking.…”
Section: Comprehensive Analysismentioning
confidence: 99%
“…Ref. [14] investigated the SSCC behavior of G105 and S135 drill pipes in simulated drilling environments containing H 2 S based on using slow-strain-rate tensile tests. Ref.…”
Section: Introductionmentioning
confidence: 99%
“…The quantitative effects of these latter chemical reactions were analyzed by the authors with a 3D FE model, where the stress concentration of the corrosion pits was estimated. In addition to the oxygen, even the H 2 S, which typically comes from the decomposition of sulfonated drilling fluid or from the environment where the drill pipe is used [27], can have a detrimental effect on the fatigue strength of drill pipe steel, as shown in Ref. [28].…”
Section: Introductionmentioning
confidence: 99%