Abstract:Fused Deposition Modeling (FDM) is a type of additive manufacturing process where prototypes are developed by depositing layers on previously deposited layer of material. Surface roughness is an important factor in determining quality of produced parts. This work proposes a methodology to calculate the surface roughness of part manufactured using FDM process. The surface roughness values to be measured using conventional stylus instrument and Digital image processing technique. Stylus comes in direct contact w… Show more
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.