The sintering, structure and properties of low-fired porcelain obtained from pastes with marshalite or marshalite with diopside replacing quartz sand are studied. The sintering temperature of porcelain made using the experimental pastes is 100°C lower (1150°C compared with 1260°C for the initial paste).