2020
DOI: 10.1007/s10904-020-01501-0
|View full text |Cite
|
Sign up to set email alerts
|

The Dual Effect of Copper and Gamma Irradiation on Chronic Wound Healing of Nanobioactive Glass

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1

Citation Types

0
3
0

Year Published

2020
2020
2024
2024

Publication Types

Select...
5
1

Relationship

1
5

Authors

Journals

citations
Cited by 12 publications
(3 citation statements)
references
References 41 publications
0
3
0
Order By: Relevance
“…Then, the suitable amounts of a series of reagents were added in the following sequence: TEP, Ca(NO 3 ) 2 •4H 2 O, and ZIF-8 nanoparticles, allowing 30 min for each reagent to react completely. The molar ratio of water/TEOS is fixed at 12/1, the ratio of H 2 O/Ethanol is 1/1, and the volume ratio of water/nitric acid is fixed at 6/1 [19]. To prevent particle aggregation, the mixture was then transferred into a standard ultrasonic bath operating at a frequency of 50-60 kHz, 100-200 W, and then, 2 M ammonia solution (a gelation catalyst) was dropped into the mixture under constant stirring.…”
Section: Preparation Of Nano Bioactive Glass (Bg)mentioning
confidence: 99%
See 1 more Smart Citation
“…Then, the suitable amounts of a series of reagents were added in the following sequence: TEP, Ca(NO 3 ) 2 •4H 2 O, and ZIF-8 nanoparticles, allowing 30 min for each reagent to react completely. The molar ratio of water/TEOS is fixed at 12/1, the ratio of H 2 O/Ethanol is 1/1, and the volume ratio of water/nitric acid is fixed at 6/1 [19]. To prevent particle aggregation, the mixture was then transferred into a standard ultrasonic bath operating at a frequency of 50-60 kHz, 100-200 W, and then, 2 M ammonia solution (a gelation catalyst) was dropped into the mixture under constant stirring.…”
Section: Preparation Of Nano Bioactive Glass (Bg)mentioning
confidence: 99%
“…The band at 1064 cm −1 refers to P-O antisymmetric stretching which could have overlapped with that of Si-O-Si asymmetric stretching, while symmetric stretching of Si-O is observed at wavenumber 797 cm −1 . The shoulder around 950 cm −1 could be related to Si-O bonds containing non-bridging oxygen (Si-O-NBO) [18,19,27]. Finally, 558 and 600 cm −1 are due to orthophosphate groups [24].…”
Section: Structural Analysismentioning
confidence: 99%
“…The scratch assay method was used to measure the migration rates of BJ.1 cells [30]. In a 24-well plate, cell density of "2 × 10 5 cells" was seeded into each well, before it was incubated at 37°C and 5% CO2 with complete medium.…”
Section: Wound Healing Activity Of Different Seeds Oils Via Wound Scr...mentioning
confidence: 99%