“…In the second experiment, 9 g of thorium was added to the mixture of 50 g tin, 1 g uranium, and 1 g calcium from the first experiment and then nitrided under 395-torr nitrogen for 2 h at a temperature of 1880 K. The nitriding rate for the thorium was found to be 6% per h. The nitriding rate of thorium in tin, in the absence of uranium, was tested using a mixture of 9 g thorium, 1 g calcium, and 50 g tin nitrided at an initial N2 pressure of [7][8][9][10][11][12][13][14][15][16][17][18] 674 torr and at a temperature of 1900 K. The nitriding was found to be nearly linear with time and was complete in 5.3 h.…”